Welding of short incisions with small depth
Welding of short incisions with small depth
Hi,
the next group of repair examples deal with larger cuts aka incisions.
In the next couple of days I will post the following repair tutorials:
- Welding of short incisions with small depth;
- Welding of short incisions with larger depth;
- Welding of longer incisions with small depth;
- Welding of longer incisions with larger depth.
The following use case is an excerpt from Indigo's handbook for the CWA .
In section V. "Application examples", part A, several repairs without material tension are showcased.
For this repair, you can use Indigo's replacement for Chinese "TPE glue", which actually is a Cold-welding TPE & TPR diffusion adhesive (CWA). This "TPE glue" alternative was developed by German company Indigo Individual, also known for a TPE repair kit, a stain remover and a magnetic M16 connector.
The example below explains how to weld a short incision with small depth.
Incisions with a length of about 2cm and a depth of about 2cm are welded in one step.
The incision is opened with thumb and forefinger:
With the brush, a very small amount diffusion adhesive is now applied and carefully distributed in the opened incision:
The incision will now be closed again with your fingers and briefly held together:
The post-processing is carried out after the curing of the diffusion adhesive. This is covered in section VI. "Post-processing" of the handbook. Every customer will receive the unabbreviated manual as PDF file.
This documentation is © by Indigo-Individual e.K., December 2018. All rights reserved.
Sandro
Metadata
Related content
Similar content as discovered by similarity of classification:
Related forum topics
Similar forum topics as discovered by similarity of classification:
Similar content
- Welding of short incisions with larger depth
- Welding of longer incisions with larger depth
- Welding of longer incisions with small depth
- ›Howto‹ repair tutorials using Indigo's CWA
- Repairing a crack in the earlobe (ripped out earring)
- Repairing a finger poke (breakthrough of a finger wire)
- Weekly summary 07/2019
- Handbooks for the cold-welding TPE & TPR diffusion adhesive
- Repairing a crack at the top of the knee with breakthrough of the joint
- Container sizes of Indigo Individual's CWA
- Indigo Individual
- Weekly summary 06/2019
- Indigo's care & repair products: Shipping to the U.S. resumed / Still long transit times
- Handbooks for the TPE repair kit ›comfort‹
- Indigo Individual closes business end of April 2021